No. |
Question |
A |
B |
C |
D |
Answer |
|---|---|---|---|---|---|---|
|
|
A weld fillet gage measures |
A. the face of the weld |
B. the throat of the weld |
C. the toe of the weld |
D. depth of fusion |
|
|
|
Undercutting is a condition that generally occurs when the |
A. welding current is too high |
B. welding current is too low |
C. welding travel speed is too slow |
D. arc length is too short |
|
|
|
During the guided bend test, when the face of the weld is on the outside of the "U", it is likely the examiner is looking for |
A. cross-sectional strength |
B. quality off fusion |
C. shearing strength |
D. degree of penetration |
|
|
|
A guided bend test specimen for mild steel is bent at an angle of _______ degrees. |
A. 45 |
B. 60 |
C. 180 |
D. 270 |
|
|
|
Refer to the picture below when answering questions 41 - 44 Identify part A ![]() |
A. face |
B. toe |
C. root |
D. leg |
|
|
|
Identify part B |
A. toe |
B. reinforcement |
C. face |
D. leg |
|
|
|
Identify part C |
A. Penetration |
B. face |
C. toe |
D. leg |
|
|
|
Identify part D |
A. toe |
B. fusion zone |
C. face |
D. leg |
|
|
|
Which of the following weld test methods would be most useful in detecting internal defects |
A. dye penetrant |
B. visual |
C. ultrasonic |
D. magnetic particle |
|
|
|
Which of the following characteristics of a weld could not be determined by visual inspection |
A. cracks |
B. dilution |
C. inclusions |
D. contour |
|